English | 
|     Chinese | 
IF SHOP 
GUESTBOOK 
IF MACHINERY WELCOME YOU!! SINCERE SERVICE FOR YOU!
PRODUCTS
IF MACHINERY TEL:0769-81888512
HotLine:13712637092
Fax:0769-81550890
Email:if89@163.com
Skype:if89if
Website:
http://www.if89.com
http://www.if-china.com
Address:Yin Chen Industrial Zone Xiao Bian village ChangAn town Dongguan City GuangDong Province china.
pad printing silicone / Welcome
Location:Home > PRODUCTS > pad printing silicone > Text
 pad printing Silicone head
 Product ID:IF-PSilicone
Description

 pad printing Silicone head  for pad printing 

 Application of  Printing Silicone rubber Pringting Effects:
Pad printing silicone rubber is used for surface printing of plastic and hardware products,and so on.
It has good resistance to wearing, no distortion, no leakage and good ink transfer property.
 
Charateristic of Transfer Printing Silicone rubber Great Pringting Effects:
pad printing silicone rubber is a double-component silicone rubber, and can be vulcanized in room temperature.
Solidify time depends on the mount of curing agent, the more the curing agent, the faster the curing.
 
Features of Printing Silicone rubber  Pringting Effects:
High print times and abrasion resistance
Without any inpurities
With good printing effects
Permanent and durable.

IF Silicone  series for pad printing head:
IFJ8368#  High-qualityColor: white|yellow |red|green Required general use
IFJ9230# Excellent-qualityColor: white|yellow |red|green Required higher use
IFJJ1800 #  Non electrostaticColor: Blue | green Required best use
Hot line:0769-81888512 。 13712637092    e-mail:if89@163.com 

 

 Operation instructions of Transfer Printing Silicone rubber Great Pringting Effects:

 1./ Firstly, prepare all the necessary tools ,like the pad mold, a cup used for mixing, a glass stick,
a wooden board with several holds and the size should be the same as the pad  


 2./ Adjust the ratio between the silicon rubber and silicon oil according to the customer’s requirement.
If customers want to print large patterns, soft silicon pad is needed and more silicon oil should be added. Otherwise,
hard silicone pad is needed, less or none silicone oil should be added.
In general, the silicone pad with 15-25 shore A is most suitable.
More silicone oil added, the silicone pad is more soft,which will lead to less printing times ,
the rising of costs and waste of raw materials. For the molecular of silicone will be destroyed by silicone oil ,
which leads to wear-resisting, solvent resistance and easy aging


3./ weight the silicon and catalyst exactly based on the ratio of 100:2.
Pls kindly note that the amount of catalyst should be the 2% of the total weight of silicone and silicone oil.


4./ weight the silicon and catalyst exactly based on the ratio of 100:2.
Pls kindly note that the amount of catalyst should be the 2% of the total weight of silicone and silicone oil.


5./ acuum pumping to de-air. The time is around 3-5 mins.


6./ 4-6 hours later, the silicone is cured completely. Get silicone pad from the mold and a printing pad is completed.

 